Blowing machine screw repair method

Update:10 10-06-2019
Summary:

1. The broken screw should be considered according to t […]

1. The broken screw should be considered according to the actual inner diameter of the barrel, and the outer diameter deviation of the new screw is given according to the normal gap of the barrel.
2. After the surface of the thread with the reduced diameter of the wear screw is treated, the wear-resistant alloy is thermally sprayed and then ground to a size. This method is generally processed and repaired by a professional spray factory, and the cost is still relatively low.
3. Surfacing the wear-resistant alloy on the threaded portion of the wear screw. Depending on the degree of wear of the screw, weld 1 to 2 mm thick and then grind the screw to size. This wear-resistant alloy consists of materials such as C, Cr, Vi, Co, W and B, which increases the anti-wear and corrosion resistance of the screw. Professional surfacing plants have a high cost for such processing, and are rarely used except for special requirements.
4.the repair screw can also be surface hard chrome plating method, chromium is also wear-resistant and corrosion-resistant metal, but the hard chrome layer is easier to fall off.